Flame Retardant
- Halogen Flame Retardant
- Phosphorus Flame Retardant
- Nitrogen Flame Retardant
- Silicon Flame Retardant
- Aluminum-Magnesium Flame Retardant
- Antimony Flame Retardant
- Boron Flame Retardant
- Expandable Graphite
- MOF Flame Retardant
- Nano Flame Retardant
- Hyperbranched Polymer Flame Retardant
-
Functional Flame Retardant
- Composite Flame Retardant for PA
- Composite Flame Retardant for PP
- Composite Flame Retardant for PBT
- Composite Flame Retardant for PVC
- Composite Flame Retardant for PU
- Composite Flame Retardant for Silicone Rubber
- Composite Flame Retardant for Epoxy Resin
- Composite Flame Retardant for TPU
- Composite Flame Retardant for TPE
- Cotton Durable Flame Retardant
- Polyester Durable Flame Retardant
- Semi-durable Flame Retardant
- Non-durable Flame Retardant
- Others
- Smoke Suppressant
- Flame Retardant Polymer
- Flame Retardant Masterbatch
UiO-66-BDC, BDC:Zr=0.66-0.98
InquiryStructure | |
Synonyms | Zirconium benzenedicarboylate |
Molecular Formula | Zr6O4(OH)4(C8H4O4)x X = 3.96-5.88 |
Appearance | White solid |
Particle Size | 0.2-0.5 μm |
Pore Volume | 0.42-0.58 cm³/g |
Size | 0.2-0.5 μm |
Specific Surface Area | 1050-1400 m²/g |
Stability | Thermal stability: 400°C; Activation temperature: 300°C |